Carbon steel hooks, spring clips and R-clips are cost-effective and highly elastic — but rust very quickly without surface protection. Zinc plating with trivalent chromium (Cr3+) passivation is the most widely used solution today, balancing corrosion resistance, cost and environmental requirements.
What is Cr3+ zinc plating?
The process consists of two main layers:
- Zinc (Zn) layer electroplated onto the steel, acting as a "sacrificial layer": the zinc corrodes first to protect the steel underneath.
- Cr3+ passivation layer over the zinc, slowing zinc oxidation and giving the surface colour (blue-white, rainbow, black).
How does Cr3+ differ from Cr6+?
| Criterion | Cr6+ passivation (traditional) | Cr3+ passivation |
|---|---|---|
| Toxicity | Cr6+ is hazardous and restricted | Much less toxic |
| RoHS / REACH compliance | Restricted | Compliant |
| Self-healing of scratches | Yes | More limited |
| Market trend | Being phased out | Current standard |
Many manufacturers exporting to the EU, US and Japan require Cr3+ so their products meet hazardous substance regulations.
Recommended coating thickness
- 5 – 8 µm: indoor parts, dry environments.
- 8 – 12 µm: parts exposed to humidity, sheltered outdoor use.
- > 12 µm: harsher environments; consider an additional sealer or switching to SUS 304.
For hooks and spring clips with threads or tight fits, the coating thickness must be considered at the design stage so the part still fits after plating.
Salt spray test
Corrosion resistance of the coating is usually evaluated by neutral salt spray testing to ASTM B117 or ISO 9227. Results are measured in hours until white rust (zinc corrosion) and red rust (base steel corrosion) appear. The required hours should be agreed in the customer's drawing or technical specification.
Hydrogen embrittlement risk with spring steel
This is the most important point when plating spring clips and R-clips:
- During acid pickling and electroplating, hydrogen atoms can diffuse into the steel.
- In high-strength steels such as spring steel, hydrogen causes hydrogen embrittlement — parts may break suddenly during assembly or under load.
- Prevention: hydrogen-relief baking (typically around 190 – 220°C for several hours) as soon as possible after plating and before passivation, following the plater's procedure.
How Hop Thai Loi coordinates plating
- Agree on plating colour, thickness and salt spray requirements at the quotation stage.
- Spring steel parts are always specified for hydrogen-relief baking after plating.
- Random checks of coverage, colour, and bend / open–close tests after plating before delivery.
- Moisture-proof packing so the coating does not develop white rust in storage.
Send us your drawing and surface requirements — we will recommend the most suitable plating option for each hook and spring clip part number.